Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.01 GPa | 437 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 3.01 GPa @Temperature -40.0 °C |
437 ksi @Temperature -40.0 °F |
ASTM D790 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 3.01 GPa @Temperature -40.0 °C |
437 ksi @Temperature -40.0 °F |
ASTM D790 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 3.01 GPa | 437 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 3.01 GPa | 437 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 3.01 GPa | 437 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Flexural Modulus | 3.01 GPa | 437 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS LNP* THERMOCOMP* AX08306 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Flexural Modulus | 3.01 GPa | 437 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS (Asia Pacific) LNP* Thermocomp* AX08306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Mineral. |
|||
Flexural Modulus | >= 3.01 GPa | >= 437 ksi | ASTM D790 |
Arlon DiClad 870 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |