Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers OpteSTAT™ NC PP 0030 Polypropylene based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas re.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® BFL2000U PC (Europe-Africa-Middle East) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | ASTM D790 |
Gichem GIBLEND F70X3/VO ABS - Polycarbonate - PC/ABS Flame Retardant
(discontinued **) Blend PC-ABS self-extinguishing class V0 high fluidity. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | ASTM D790 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | ASTM D790 |
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX1127 PPE+PS Automotive electrical applications. 250F (120C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2mm/min; ISO 178 |
Denka MALECCA K-095 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2mm/min; ISO 178 |
Denka MALECCA K-200 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6240 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |