Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.41 GPa | 350 ksi | Tangent; ASTM D790 |
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers PC-1011 L Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS Color Package may affect performance. Visual Fx PC+ABS in various metallic (Ares) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Flexural Modulus | 2.41 GPa @Thickness 3.17 mm |
350 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.41 GPa @Thickness 3.17 mm |
350 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
PolyOne Lubri-Tech™ ATH-000/20T Homopolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
PolyOne Lubri-Tech™ NL-15GM/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
M. Holland Company PC518R Polycarbonate High clarityUltra high impact resistanceGood mold releaseApplications: AppliancesFood containersTable products |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
LG Chemical Lupoy 1200-08 Polycarbonate Resin Description: LUPOY PC 1200-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER LNP* LUBRICOMP* KP004AXZ is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 407 L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Star Plastics PC743 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS LG UV Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Star Plastics ABS448T Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Styron CALIBREâ„¢ 303-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Formosa Plastics Formolon® APW Compound APW Powder Window Profile Compound Series The APW compounds have been designed for profile extrusion in window lineals, fencing and other outdoor weatherable markets. It exhibits excellent whiteness.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | Tangent; ASTM-D790 |
CTC X-PRO CF 40 6002XT Polypropylene Copolymer, 40% Calcium Carbonate Filled X-PRO CF 40 6002 XT is a heat stabilized, 40% calcium carbonate filled polypropylene copolymer. It has an application in extrusion.Data provided by Composite Technologies (CTC). |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D-790 |
CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board REN SHAPE 5008 is a tooling board specifically designed for use in vacuum forming. It is designed for use up to 250°F and is well suited for building vacuum forming molds as well as master models,.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | Tangent; ASTM D790 |
RheTech Products HP506-01B 22% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |