Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.40 GPa | 348 ksi | ASTM D790 |
Nylene® Norpex® AX290 PPE (Polyphenylene Ether); High Performance High Heat Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East) CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® RCY6214 PC+ABS (Asia Pacific) Cycoloy* RCY6214 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1.5 mm. D.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178 |
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PH 91 T 20 Polypropylene Homopolymer, 20% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178 |
Solvay Engineered Polymers SEQUEL® 2382 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2382 engineered polyolefin is designed for large mold-in-color interior applications that require stiffness and dimensional stability. This material exhibits excellent process.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ASTM D790 |
LG Chemical Lupoy 3030-10 Polycarbonate Resin Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ASTM-D790 |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178 |
Mitsubishi Xantar® 27 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178 |
Mitsubishi Xantar® FC 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178 |
Mitsubishi Xantar® MX 2042 FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | DIN 53457 |
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Conditioned Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 3-point; ISO 178 |
Styron CALIBREâ„¢ 302V-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300V Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are availab.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178-93 |
Wellman Wellpet® PR118-N2 Unfilled Polyester PET Description: Unfilled Polyester PETInformation provided by Wellman. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178 |
Total PS CPDS 827 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 827 is a high impact flame retardant polystyrene for use in HGW applications. PS CPDS 827 can be supplied in both natural and colored forms.Main Characteristics:DBD.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ISO 178 |
Hexcel® HexPly® 108 180°C Curing Epoxy Matrix HexPly® 108 is a high temperature resistant epoxy resin system developed for the fabrication of primary aircraft and space structures. 108 has excellent hot wet properties and exhibits low viscosit.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 2 mm/min; ISO 178 |
Covestro Makrolon® FU1007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ASTM D790, ISO 178 |
EPICHEM Epiryl B PPO Polyphenylene oxide |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | dry; ISO 178 |
DSM EcoPaXX® Q-X07290 PA410-I Impact Modified |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | 2 mm/min; ISO 178 |
Chi Mei Wonderlite® PC-110N Polycarbonate - Flame Retardant Opaque |
|||
Flexural Modulus | 2.40 GPa | 348 ksi | ASTM D790 |
Ashley Polymers Ashlene® 1513 Polycarbonate A rigid flame retardant polycarbonate, UV stabilized in black for applications requiring superior dimensional stability and overall toughness.Data provided by the manufacturer |