Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.86 GPa | 270 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Hyosung Topilene J700-1 PP J700-1 Injection Special Purpose GradeApplications:Disposable syringeHouseware applianceCharacteristics:Slip propertyHigh stiffnessFast cycleInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.86 GPa @Thickness 3.20 mm |
270 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID HI1202B(W) PA66, High Impact Feature: Injection Molding, PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333HI2 High Impact Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D570 |
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0141 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Lendell Parapet GR-00100 PMMA, High Impact |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
2.5mm/min; ASTM D790 |
LG Chemical Lupox® TE5011 PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Spartech Soft Touch R-104 Laminated Sheet Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® ES-0173 ABS, Extrusion Grade Extrusion ABS for the interior of refrigerator with HCFC-141b, down gauging characteristicInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D 790 |
Styrolution PS 5600/5601 HIPS Fine balance of toughness and rigidityGood processabilityUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Samyang Trimma® SD6320P PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6 E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 364 PBT Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.86 GPa @Thickness 3.20 mm |
270 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 555 Flame Retardant Polystyrene Characteristics Very good flow properties Good balance of toughness and rigidity Available in any dark colors Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxe.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 4142R Injection Molding Polypropylene Homopolymer with Nucleating, Antistat AdditivesApplications: Appliance, closure and thin wall applications.Formolene 4142R is a low viscosity, highly isotactic polypropylene homopolymer designed pri.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790, ISO 178 |
Ensinger TECAPRO™ SAN Polypropylene (PP) TECAFORM™ (Polyacetal) and TECAPRO™ SAN (Polypropylene), provide an additional safety factor in reducing incidence of bacterial contamination. The raw materials are charged with an antimicrobial .. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 9502E Description: Extrusion Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Aaron Industries AAROPRENE® CFPP 2010 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP CL001I PS LNP* Lubricomp* CL001I is a compound based on Polystyrene resin containing 5% PTFE. Added features of this material include: Internally Lubricated, High Impact. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc. |