Polymer Property : Flexural Modulus = 252 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.74 GPa
252 ksi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ AT-000/18T 2S Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Modulus 1.74 GPa
252 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Solvay Engineered Polymers SEQUEL® 1823 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 1823 engineered polyolefin is designed for automotive exterior applications that require energy management combined with excellent ductility and stiffness over a broad temperat..
Flexural Modulus 1.74 GPa
252 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Flexural Modulus 1.74 GPa
252 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Flexural Modulus 1.74 GPa
252 ksi
2 mm/min, 64mm span; ISO 178
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP
SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin..
Flexural Modulus 1.74 GPa
252 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
SABIC Innovative Plastics NORYL CRX1005 PPE+HIPS (Asia Pacific)
PPE+PS Chemical resistance improved
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion
DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized..
Flexural Modulus 1.74 GPa
252 ksi
1.3 mm/min, tangent; ASTM D790
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Flexural Modulus 1.74 GPa
252 ksi
1.3 mm/min, tangent; ASTM D790
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Flexural Modulus 1.74 GPa
252 ksi
1.3 mm/min, tangent; ASTM D790
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
Tipco Tipcolene® FPW 10 PPC - 10% Wollastonite Reinforced Polypropylene Copolymer, High Impact Strength
10% Wollastonite Reinforced PP CopolymerApplications: Automotive & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion
DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized..
Flexural Modulus 1.74 GPa
252 ksi
1.3 mm/min, tangent; ASTM D790
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Flexural Modulus 1.74 GPa
252 ksi
1.3 mm/min, tangent; ASTM D790
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion
DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized..
Flexural Modulus 1.74 GPa
252 ksi
1.3 mm/min, tangent; ASTM D790
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion
DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized..
Flexural Modulus 1.74 GPa
252 ksi
ISO Data
BASF Ultraform N 2640 Z4 BK140 Q600 POM
Ultraform N2640 Z4 BK140 Q600 is a high toughness, elastomer-modified injection molding POM grade.
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion
DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized..
Flexural Modulus 1.74 GPa
252 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics NORYL FN150X PPE+PS
Improved reliability and productivity. Thin wall capability. UL94 V-0/5VA rated. All data at 20% weight reduction and 0.250"" wall.
Flexural Modulus 1.74 GPa
252 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 1024E-01 Olefinic Elastomer For Sheet Extrusion
DescriptionPolytrope TPP 1024E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized..
Flexural Modulus 1.74 GPa
252 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon MDM40 PP
LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region.