Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Multibase Multi-Pro® 2516 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | Tangent; ASTM D790 |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | >= 1.65 GPa | >= 240 ksi | ASTM D790 |
S&E Specialty Polymers GPP6025 PP Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus .. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-1503 G10 Description: Glass Reinforced PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Network Polymers Nylon 6615 L Description: Black Super Tough NylonInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.65 GPa @Thickness 3.20 mm |
240 ksi @Thickness 0.126 in |
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A |
Pinnacle Polymers 1220 Polypropylene Homopolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Flexural Modulus | 1.65 GPa @Thickness 3.20 mm |
240 ksi @Thickness 0.126 in |
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A |
Pinnacle Polymers 1508 Polypropylene Homopolymer, Fiber Spinning Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Flexural Modulus | 1.65 GPa @Thickness 3.20 mm |
240 ksi @Thickness 0.126 in |
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A |
Pinnacle Polymers 1704 Polypropylene Homopolymer, Stretched Tape Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ 383 ASA
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 1.65 - 6.21 GPa | 240 - 900 ksi | Average value: 1.94 GPa Grade Count:18 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (Cond)
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 1.65 GPa @Temperature 23.0 °C |
240 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H35Z-00 Polypropylene Homopolymer This is a high flow rate, nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 C.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | secant; ASTM D790 |
Spartech PP5230 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Techmer ES Statiblend® ABS FR AS BN Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | 1% Secant; ASTM D790 |
Washington Penn Homopolymer Polypropylene 10% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem FF450WV Homopolymer Polypropylene Description: Excellent Processability, Nucleated.Applications: Suggested Uses Include Fast-Cycle Injection Molding and CompoundingProcess: Injection Molding.This resin meets the requirements for ole.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Asahi Kasei Thermylene® P-05FG-0870 5% Glass Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem H521 Homopolymer Polypropylene Description: Injection Molding, General Purpose, Low Water CarryoverApplications: Suggested Uses Include Tape, Slit-film Fibers, Containers, Closures, HousewaresThis resin meets the requirements for.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Amco PRIMATOP HDPE 006964EG Pipe Extrusion Polyethylene HDPE 006964 features high quality for critical food packaging requirements and excellent stiffness. Applications include milk, water, and juice packaging.Former A-Top Polymers product; part of Amco .. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | Tangent; ASTM D790 |
RheTech Products CC20P100-00 20% Calcium Carbonate Reinforced Polypropylene, Natural Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.65 - 2.45 GPa | 240 - 355 ksi | Average value: 2.08 GPa Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |