Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790 |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers SEQUEL® 1490 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1490 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790A |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1% Secant; ASTM D790 |
Flint Hills P4G3Z-050 Homopolymer Polypropylene Homopolymer, FDA compliant.Features: Low water carryover.Applications: Extrusion: slit film and oriented fibers.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1% Secant; ASTM D790 |
Flint Hills P4G4B-036 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated, antistat, and drug master file 9988.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now .. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790A |
Ineos H01G-00 Polypropylene Homopolymer Grade H01G-00 is a polypropylene homopolymer for fiber, tape, and consumer applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.152.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1% Secant at 0.05 in/min; ASTM D790 |
Ineos H03W-01 Polypropylene, Gas Phase Polymerized H03W-01 (formerly Fortilene® HG3253) belongs to the new generation of polypropylenes produced by gas phase polymerization. This nominal 4 melt flow index product is specifically designed for fib.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790A |
Ineos H13M-00 Polypropylene Homopolymer Grade H13M-00 is a general purpose polypropylene homopolymer for injection molding applications. It provides good long-term heat stability.Suggested fabrication methods: Injection moldingFeatures: .. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790 |
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790 |
Engineered Plastics EPABS 19 ABS Extrusion Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1.0 in/min; 0.125" thickness; ASTM D-790 |
Chevron Phillips K-Resin® KR03BR SBC
(discontinued **) K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:BottlesMolded boxes and containersMedical devicesPortion packagesBlister packagingFeatures:Good stiffnessGood formabilityGood toughnessExcelle.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790 |
Braskem H 606 Thermoforming Polypropylene Description: H 606 is low melt flow rate homopolymer with general purpose additive package. This resin is designed for extrusion and thermoforming. H 606 presents excellent processability and high o.. |