Mechanical Properties Metric English Comments
Flexural Modulus 1.44 GPa
209 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Modulus 1.44 GPa
209 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Modulus 1.44 GPa
209 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Modulus 1.44 GPa
209 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly
LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic.
Flexural Modulus 1.44 GPa
209 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.
Flexural Modulus 1.44 GPa
209 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal
LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat.
Flexural Modulus 1.44 GPa
209 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-LOY M3000 PP
LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat.
Flexural Modulus 1.44 GPa
209 ksi
Zylog Hipolyene® 1046 NM Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.44 GPa
209 ksi
ASTM D790
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System
0.1 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offi..
Flexural Modulus 1.44 GPa
209 ksi
50%RH; ISO 178
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Flexural Modulus 1.44 GPa
209 ksi
50%RH; ISO 178
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Flexural Modulus 1.44 GPa
209 ksi
50%RH; ISO 178
DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Flexural Modulus 1.44 GPa
209 ksi
.5"/min; CP-TM-10
PolyOne Elastamax HTE 2101-1002 Polyurethane Alloy  (discontinued **)
This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. ..