Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES Electrafil® J-4/25/CF/15 BK PA6/12 |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES Electrafil® J-4/25/CF/15 NAT PA6/12 |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 L LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: Natural ColorInf.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedInformation provided by TP C.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 X 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composit.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composit.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 X LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Com.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF55 HS L 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PA6 LGCF50 HS BK 6mm 50% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAp.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PPS GF40 TL13 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES Luriblend® PPS/F GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackIn.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East) LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6 GF/M50 FR 50% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Techmer ES HiFill® PPS GF40 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RVL29 PA 66 LNP VERTON* RVL29 is a compound based on Nylon 66 resin containing 45% Long Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Structural. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RVL29 PA 66 (Asia Pacific) LNP VERTON* RVL29 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Plenco 6343 Phenolic, Granular, Transfer Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Asahi Kasei Thermylon® NSG-440A 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis.. |
|||
Flexural Modulus | 14.1 GPa @Temperature 90.0 °C |
2050 ksi @Temperature 194 °F |
ASTM D790 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RVL29XXP PA 66 (Europe-Africa-Middle East) LNP VERTON* RVL29XXP is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |