Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.35 GPa | 196 ksi | |
Plastcom SLOVALEN PC 18 FRT 5 PP, mod. of mech. properties, fire retardant FeaturesModified copolymer PP for extrusion, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Delivered in natural mode and in the full RAL colour sc.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | Tangent; 1.3 mm/min; ISO 178 |
Mytex Polymers AS33L-16 Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33L-16 is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and goo.. |
|||
Flexural Modulus | >= 1.35 GPa | >= 196 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1450R (Z30S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | >= 1.35 GPa | >= 196 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1500L (C30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Radici Radilon® AUSX200 (dry) Nylon 66 Very high impact strengthInformation provided by Radici group. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | Tangent, 1.3 mm/min; ASTM D790 |
Flint Hills P6G2N-095 Impact Copolymer Polypropylene Features: Excellent stiffness and impact resistance, nucleated, suitable for retort and hot fill applications. Product does not contain animal derived components.Applications: Blow molding, sheet/.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790 |
Iran Petrochemical (PCC) 52518 High Density Polyethylene 52518 is a HDPE copolymer for injection molding applications requiring a good balance between easy of process, flow and mechanical properties. Application: housewares, high fluidity, injection moldi.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Iran Petrochemical (PCC) D 50 S Polypropylene Moplen D 50 S is a homopolymer with a high molecular weight and outstanding mechanical properties. The product shows excellent processability in extrusion applications and exhibits excellent long te.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790 |
Teknor Apex Sinpolene CPP2020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 20% Filler by Weight Features: Copolymer Uses: Furniture Forms: PelletsInformation Provided .. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | 2mm/min; ISO 178 |
Borealis Daploy™ WB180HMS Polypropylene Daploy™ WB180HMS is a propylene-based, structurally isomeric polymer.Information provided by Borealis AG |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | 5mm/min; ISO 178 |
Borealis HD204CF Polypropylene HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Unipetrol PP MONSTEN® MA 745 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790 |
Total PPC 5720WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very .. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Total PPH 4054 Polypropylene Homopolymer Polypropylene PPH 4054 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4054 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPH 4060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4060 is homopolymer.ApplicationATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | At 1 mm/min; ISO 178 |
Borealis Borstar® BB2581 HDPE for Blow Molding Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for h.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
ExxonMobil PP1063L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790A |
Dow 5E16S Polypropylene Homopolymer Resin OverviewConsistent processabilitySuperior impactGood mold releaseContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aComplies with Canadian HPFB No ObjectionDOW 5E16S Polypr.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790A |
Dow H533-35RGU Polypropylene Homopolymer Resin OverviewExcellent spinnabilityConsistent processingAnti-gas-fadingUV resistantComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW H533-35RGU Polypropylene Resin is a controlled rheology grade intended.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 527 |
Dow INSPIRE™ 112 Performance Polymer INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® LE 60 SF Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | SAE J949 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ASTM D790 |
Carmel Olefins CAPILENE® T 12 EV Polypropylene Homopolymer CAPILENE® T 12 EV is a polypropylene homopolymer with narrow molecular weight distribution, controlled rheology, intended for fiber applications. It is characterized by easy processing, very good m.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, Conditioned Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | 1% secant; ASTM D790 |
Braskem H 603 Blow Molding Polypropylene Description: H 603 is a low melt flow rate homopolymer used for general purposes. This resin is designed for blow moulding and extrusion applications. H 603 exhibits excellent processability, excell.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
Polimeri Europa Eraclene® MM 84 U High Density Polyethylene - Injection Molding Eraclene MM 84 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 U is characterized by high rigidity and good impac.. |
|||
Flexural Modulus | 1.35 GPa | 196 ksi | ISO 178 |
ExxonMobil PP1364E2 Polypropylene Homopolymer Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc.. |