Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Oxford Polymers PPS/66-505-40GF-BK PPS/PA66, 40% Glass Fiber Reinforced Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy with Nylon 66 Processing and Delivery Form: Pellets and Injection MoldingAppearance: Bla.. |
|||
Flexural Modulus | 12.7 GPa @Thickness 3.20 mm |
1850 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 5 mm/min; ISO 178 |
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF25 BK 25% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 25% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF60 BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF60 LE 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 IM 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingIn.. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | |
Shinil Chemical SHINCON PEI-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF20 TL15 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance:.. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF20 TS15 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAdditive: PTFE Lubricant(10%) and Silicone Lubricant Features: Lubricated, Good Wear Resistance and L.. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF30 TS15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Silicone LubricantFeatures: Lubricated, Low Friction and Good Wear .. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140 PPS Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140C PPS Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES Electrafil® J-1200/CF/30 ABS, 30% Carbon Fiber Reinforced |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.8 GPa @Temperature 22.8 °C |
1850 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G8-43GF Nylon 66, 43% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140 PPS Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140C PPS Information provided by Samsung Cheil Industries. |