Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent; ASTM D790 |
RheTech Products FT4650-01UV Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent; ASTM D790 |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent; ASTM D790 |
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | tangent; ASTM D790 |
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO PP, Flame Retardant Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | tangent; ASTM D790 |
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO-15 PP, Flame Retardant Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 25-3701 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-4IMP Impact Modified Nylon 66 for Injection Molding Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790A |
Dow INSPIRE™ TF1302 TPO
(discontinued **) Medium Flow, High Impact, Filled TPOInformation provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Formosa Plastics Formolene® LH6008 Injection Molding HDPE
(discontinued **) HomopolymerApplications: Totes, cases, crates, over-caps, toysFormolene LH6008 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Admi.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM350LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding COPYLENE™ CM350LN is a high melt flow, controlled rheology, medium impact polypropylene copolymer resin designed for injection molding applications requiring a good balance of stiffness, impact, re.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
M. Holland Company CP200 Polypropylene Impact Copolymer Impact copolymerMedium impact resistanceLow temperature impact resistanceApplications: Appliance componentsConsumer ApplicationsHousehold goodsInformation provided by M. Holland |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP500 Polypropylene Copolymer Features: High Flow, High Impact Resistance, Good StiffnessUses: Automotive, Interior Parts Closures, Household Goods, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformati.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 1% Tangent, 1.27 mm/min; ASTM D790 |
I. Stern 3335 Prime Impact Copolymer Polypropylene Features:Superior color and process stabilityLow odor, good flow and set up behaviorExcellent see through clarityApplicationsReusable food containersHousewaresPackagingInformation provided by I. Ste.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent-Method 1; ASTM D790 |
Ineos T50-1000 HDPE Copolymer T50-1000 is a high density polyethylene copolymer. It has a narrow molecular weight distribution and provides injection molded parts with an excellent balance of properties and processing for most g.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Luriblend® PA4/6 HS TL15 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc... |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Luriblend® PA4/6 TL15 HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D709A |
Styron INSPIREâ„¢ TF1302 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Electrablend® PA12 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES HiFill® HDPE Availability: North AmericaForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D 790 |
Total 50100.1 HDPE blow molding Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging. Blow Molding Stock Temperature 370 – 450 ºF Extrusion melt tempera.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AB50-003 Blow Molding Resin Product Description: AB50-003 is a blow molding grade high density polyethylene copolymer. This resin has very good stress crack resistance combined with high impact strength and rigidity.Availabili.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | |
Dow HDPE 30460M High Density Polyethylene DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4007G Impact Copolymer Polypropylene Description: Extra high izod impact, superior low temperature drop impact.Applications: Suggested uses include profiles, tubing, squeeze bottles. UL temperature index of 100ºC.Process: Injection Mo.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4015F Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the .. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Amco PRIMATOP HDPE 080960 Injection Molding Polyethylene HDPE 080960 features high stiffness, maximum toughness, good top loading capability, and high surface gloss. Applications include tote boxes and beverage crates.Former A-Top Polymers product; part o.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Luriblend® HDPE GL5 Availability: North AmericaForms: PelletsAdditive: Graphite Powder LubricantInformation provided by TP Composites, Inc. |