Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.110 GPa | 16.0 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE G 7150 BLK Multi-Flex® G 7150 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactu.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Flex® TPO D-3120 Multi-Flex® TPO D-3120 is a compound for automotive applications replacing Himont's 7023. The burn rate is 0.87 in/min; ASTM FM VSS 30.Data provided by Multibase. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ISO 178 |
Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection mo.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ISO 178 |
Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection moldi.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ISO 178 |
Polimeri Europa Riblene® MV 10 R Low Density Polyethylene - Injection Molding Riblene MV 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 R are highly flexible.Main Applications: Riblene MV 10 R is ideal for injection.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ASTM D790 |
Rotuba MH Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ISO 178 |
Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for inject.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ASTM D790 |
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Adflexâ„¢ KS-084P TPO Resin Primary Processing Method: ExtrusionKey Features: high melt flow, low modulus, impact resistant thermoplastic olefin, resin, good heat sealability, outstanding puncture resistance, excellent balance.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific) Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific) Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD801AU PPE-TPE (Asia Pacific) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ASTM D790 |
Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ASTM D790 |
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ASTM D790 |
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ASTM D790 |
DuPont Keldax® 6798 Filled Thermoplastic Ethylene Polymer A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ASTM D790 |
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | |
Dow AFFINITY™ SM 1300 Polyolefin Plastomer AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closu.. |
|||
Flexural Modulus | 0.110 GPa | 16.0 ksi | ASTM D790 |
3D Systems VisiJet M100 3-D Printer Model Material The InVision SR (standard resolution) 3-D printer delivers key advantages compared to other 3-D modeling technologies — superior model quality, durable photopolymer materials, surface finish and fe.. |