Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined by UL 1581. 87 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Melt Flow 7.5 g/10 min

@Load 5.00 kg,
Temperature 250 °C
7.5 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
30S reading; ASTM D2240
Tensile Strength at Break 19.0 MPa
2760 psi
50 mm/min; ISO 527
20.0 MPa
2900 psi
Type I, 50 mm/min; ASTM D638
28.0 MPa
4060 psi
UL 1581
30.0 MPa
4350 psi
after 7days @136°C; UL 1581
Elongation at Break 132 %
132 %
50 mm/min; ISO 527
146 %
146 %
Type I, 50 mm/min; ASTM D638
200 %
200 %
after 7days @136°C; UL 1581
240 %
240 %
UL 1581
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.110 GPa
16.0 ksi
12.5 mm/min; ISO 178
Tear Strength 7.50 kN/m
42.8 pli
ISO 6383
Heat Distortion 14 %

@Load 0.250 kg,
Temperature 121 °C
14 %

@Load 0.551 lb,
Temperature 250 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Oxygen Index 24 %
24 %
ISO 4589
Glow Wire Test 725 °C
1340 °F
IEC 60695-2-13
750 °C

@Thickness 3.00 mm
1380 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+16 ohm-cm
1.90e+16 ohm-cm
ASTM D257
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm

@Thickness 2.00 mm
635 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0068

@Frequency 1.00e+6 Hz
0.0068

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 102
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 66
ASTM E 662
VW-1 Pass
UL 1581
Copyright © lookpolymers.com All Rights Reserved