Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
PolyMirae Moplen EP300C Sheet and Thermoforming Grade Polypropylene Moplen EP300C is the polypropylene blockpolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300C is a block copolymer particularly suitable for sheet and t.. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
PolyMirae Moplen EP400M Injection Molding Grade Polypropylene Moplen EP400M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP400M is a block copolymer selected by customers for use in in.. |
|||
Flexural Modulus | 1.08 - 27.5 GPa | 156 - 3990 ksi | Average value: 10.6 GPa Grade Count:34 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
PolyMirae Moplen EP300H Injection Molding Grade Polypropylene Moplen EP300H is a heterophasic copolymer, suitable for injection moulding as well as for thermoforming applications. Moplen EP300H is a excellent low temperature impact behavior combined with a goo.. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
PolyMirae Moplen EP332C Pipe Extrusion Grade Polypropylene Moplen EP332C is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP332C is a block copolymer appreciated by customers in the mar.. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
Hyosung Topilene B240LP PP B240LP Extrusion Impact CopolymerApplications:Extrusion blow moldingCharacteristics:High impactHeat stabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
Hyosung Topilene C600 PP C600 Film Grade Butane Random CopolymerApplications: Metallizing CPPCharacteristics:Al bonding strengthHigh glossInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
Hyosung Topilene R601 PP R601 Injection Random CopolymerApplications:High transparent productISBM bottleCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.08 GPa @Thickness 6.40 mm |
156 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL TE5108H PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | Olsen Stiffness; ASTM D747 |
Global B-5200 High Density Polyethylene Description-has excellent stiffness thus requires less material to make
blow moldingApplications-food containers, drinking bottles, medicine bottles, water containersInformation provided by Global .. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | Olsen Stiffness; ASTM D747 |
Global J-2208 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
LG Chemical LUTENE-H PE0235 HDPE Description: LUTENE-H PE0235 is a materials with high toughness and rigidity suitable for cable protection It has very high resistance to stress cracking and long-term internal pressure creep proper.. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | 5 mm/min; ISO 178 |
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | 5 mm/min; ISO 178 |
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
LG Chemical LUTENE-H ME6000 HDPE Description: LUTENE-H ME6000 is mainly intended for injection molding of crates. It has excellent mechanical properties and high impact strength.Applications: Transport and stacking crates, bottle c.. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GP-5400G PBT, 40% Glass Filled Material with 40% GF reinforcement that is used in motor insulatorsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GP-5400G PBT, 40% Glass Filled Material with 40% GF reinforcement that is used in motor insulatorsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 1.08 GPa | 156 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 1.08 GPa @Thickness 3.20 mm |
156 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 8001 High Gloss, ESCR High Impact Polystyrene Characteristics Very high toughness Excellent ESCR properties against common food chemicals High gloss & heat resistance Processing Extrusion & Forming Applications Fatty food containers Co-extru.. |