Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.07 GPa | 155 ksi | Chord; 2 mm/min; ISO 178 |
Mytex Polymers AS78L(W)-GM-02 Polypropylene, Rubber modified, Compounded Description: AS78L(W)-GM-02 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties.Key Applications: Bumper fascias and all other exterior partsInform.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent; ASTM D790 |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-1002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 50-0350 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2807 HDPE Injection Molding Resin Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Industrial and lubricant pails.Data provided by .. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2815 HDPE Injection Molding Resin Features: Excellent balance of stiffness and toughness, low odor.Applications: Margarine and spreads, thin walled containers, frozen food containers.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
Petromont 4100 High Density Polyethylene Resin Petromont HDPE 4100 is a high density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is designed for general use in large diameter heavy duty and non pressure pipe
appl.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
Formosa Plastics Formolene® LH5206 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lidsFormolene LH5206 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as specified in 2.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM015 Polypropylene Impact Copolymer COPYLENE™ CM015 is low melt flow impact copolymer with a barefoot additive package and is designed for excellent processing in injection molding and extrusion applications.Applications: Injection M.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® C513UV HDPE Blow Molding Resin
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Outstanding impact resistanceExcellent ESCRExcellent processabilityUV stabilizationApplications: Intermediate bulk containersAgricultural containersInfor.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP502 Polypropylene Copolymer Features: Copolymer, High Flow, High Impact ResistanceUses: Closures, Medical Applications, Thin-walled PartsProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
M. Holland Company CP510 Polypropylene Copolymer Additives: Heat Stabilizer, Nucleating AgentsFeatures: High Flow, High Impact Resistance, Heat Stabilizer, NucleatedUses: Construction Applications, Lawn and Garden EquipmentApprovals: FDA 21 CFR 17.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1% Tangent, 1.27 mm/min; ASTM D790A |
I. Stern 3320 Prime Impact Copolymer Polypropylene Features:Excellent balance of stiffness and impact strengthExcellent long term aging propertiesExcellent color and process stabilityApplicationsClosuresHousewaresSmall appliancesLawn and GardenInfor.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PCC 4414 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2510W Medium Impact Copolymer Polypropylene Impact CopolymerApplications: Trans-white battery casesFormolene 2510W is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dime.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2575N injection Molded Polypropylene Impact Copolymer for High Speed injection Molded ApplicationsFormolene® 2575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging, .. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6600A Impact Copolymer Polypropylene Impact Copolymer for Extrusion and Compounding Applications (Fractional Melt Flow) Formolene® 6600A is a high impact copolymer with an excellent balance of toughness and stiffness. It is suitable f.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 3312B Random Copolymer Polypropylene Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3312B is a medium melt flow random copolymer with fast cycle time and easy mold release. It is designed for injection moldin.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin Resin Type: Hexene CopolymerCharacteristics: Moderate flowExcellent impact strengthExcellent ESCRGood warpage resistanceApplications: Industrial partsSeatsFood and household containersAgricultural p.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® 9503H HDPE Blow Molding Resin Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRExcellent impact resistanceApplications: Detergent bottlesIndustrial containers/large partsHousehold and industrial chemical containersIn.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent; ASTM D790 |
Chevron Phillips Marlex® C513UV High Density Polyethylene, Blow Molding This extra high molecular weight, hexane copolymer is tailored for intermediate bulk container applications that require:Outstanding impact resistanceOutstanding ESCRExcellent processabilityUV stabi.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
Dow C719-35RNHP Polypropylene High Impact Contains nucleating agent Controlled rheology product Complies with U.S. FDA 21 CFR 177.1520 © 3.1a Information provided by DowDow Announced Sale of Global Polypropylene Business to B.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1% Secant; ASTM D790A |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow 6D83K Polypropylene Resin DOW 6D83K is intended for use in extrusion blow molding processes where enhanced clarity is desired.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July .. |
|||
Flexural Modulus | >= 1.07 GPa | >= 155 ksi | ASTM D790 |
Buckeye Polymers BP PPC 0212 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TR3120C Random Copolymer Polypropylene Description: Superior color and processing stability, low odor, good flow and set-up behavior, excellent see through clarity.Applications: Suggested uses include housewares, reusable food containers.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM015G Polypropylene Impact Copolymer COPYLENE® CM015G is low melt flow impact copolymer with a barefoot additive package and is designed for excellent processing in injection molding and extrusion applications.Applications:Injection M.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
Amco PRIMATOP HDPE 055952 Injection Molding Polyethylene HDPE 055952 features maximum toughness, good top loading capability, and high surface gloss. Applications include pails and beverage crates.Former A-Top Polymers product; part of Amco product line s.. |