I. Stern 3320 Prime Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer I. Stern & Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern 3320 Prime Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features:Excellent balance of stiffness and impact strengthExcellent long term aging propertiesExcellent color and process stabilityApplicationsClosuresHousewaresSmall appliancesLawn and GardenInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3300 psi
51 mm/min; ASTM D638
Elongation at Yield 12 %
12 %
51 mm/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
1% Tangent, 1.27 mm/min; ASTM D790A
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256