Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Oxford Polymers 40GF 40% Glass Fiber Filled Polycarbonate for Injection Molding 40% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 9.67 GPa | 1400 ksi | ASTM Data |
BASF Capron® SEG7 35% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron SEG7 is an unfilled injection molding type 6 nylon graft copolymer. It has superior impact resistance and flow especially for thinner walled parts and long flow lengths. Copolymerization res.. |
|||
Flexural Modulus | 9.65 - 11.0 GPa | 1400 - 1600 ksi | ASTM D790 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | Flexural 0.5% Secant Modulus; ASTM D790 |
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM AR9300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF33 TL15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF50 ML2 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: BlackUL File Num.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 HS L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF33 ML2 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: LubricatedInformation provided by TP Composites,.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+PS LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses). |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 9.65 - 11.0 GPa | 1400 - 1600 ksi | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Techmer ES Luriblend® PPA GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low .. |