Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.910 GPa | 132 ksi | 1% Secant; ASTM D790 |
ExxonMobil HD 6761.17 Injection Molding Resin
(discontinued **) HD 6761 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a heavy-d.. |
|||
Flexural Modulus | 0.910 - 147 GPa | 132 - 21300 ksi | Average value: 13.8 GPa Grade Count:136 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | 2mm/min; ASTM D790 |
Kingfa PA6-MG45 45% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GF 4950 HS HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 5250 OC HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H5211PBR High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Non pressure pipes, co-extruded pipes as the inner layerInformation provided by SCG Chemicals |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Flexural Modulus | 0.911 GPa | 132 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Flexural Modulus | 0.911 GPa | 132 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Flexural Modulus | 0.911 GPa | 132 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Flexural Modulus | 0.911 GPa | 132 ksi | ASTM D790 |
Toyobo PELPRENE™ S9002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Flexural Modulus | 0.911 GPa | 132 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.911 GPa | 132 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.911 GPa | 132 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren.. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | |
Dow DOWLEX™ IP-40 High Density Polyethylene DOWLEX® IP-40 resin is an improved processing high density resin designed to offer excellent processability and impact resistance required for food container applications. This resin is designed by.. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | |
Dow DOWLEX™ IP-90 High Density Polyethylene Next Generation DOWLEX® IP-90 resin is a high flow improved processing high density polyethylene resin designed for ultra-thin wall injection molded containers and drink cups. This resin has been m.. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Flexural Modulus | 0.910 GPa | 132 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXFLEX® 930HS TPO
(discontinued **) Description: DEXFLEX® 930HS is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope.. |