Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.772 GPa | 112 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-1010 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-2010 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | ASTM D790 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.772 - 1.17 GPa | 112 - 170 ksi | Average value: 0.903 GPa Grade Count:12 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | 2% Secant; 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | |
Dow HDPE 42047N High Density Polyethylene DOW HDPE 42047N resin is a narrow molecular weight distribution copolymer designed to combine high impact strength and environmental stress crack resistance with excellent processability over a wide.. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | ISO Data |
BASF Ultramid® 8202 HS BK-102 PA6 (Conditioned) Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses .. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | ISO Data |
BASF Ultramid® 8202 HS PA6 (Conditioned) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Modulus | 0.770 GPa | 112 ksi | ISO Data |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Flexural Modulus | 0.770 GPa @Temperature 93.0 °C |
112 ksi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Dry) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | ASTM D790 |
Lucent Polymers TPO-10T Thermoplastic Polyolefin, 10% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **) LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili.. |