Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 6.20 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.40 - 6.20 GPa
783 - 899 ksi
Longitudinal
Quadrant Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite
MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. Howev..
Flexural Modulus 1.10 - 6.20 GPa
160 - 899 ksi
Average value: 2.50 GPa Grade Count:12
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Flexural Modulus 2.10 - 6.20 GPa

@Temperature -40.0 - 120 °C
305 - 899 ksi

@Temperature -40.0 - 248 °F
Average value: 3.79 GPa Grade Count:5
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..