Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
PolyOne Nymax™ GF 1200 33 Red 31 A Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Nylene® 9633 , 33% Glass Reinforced Nylon 6,6/6 Description: Nylene® 9633 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resou.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Niche Polymer PA6GF33BK Nylon 6, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Niche Polymer PA6GF33N Nylon 6, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1240MGHL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement -15% Filler by Weight, Mineral -25% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat S.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2233HL BK Nylon 6 Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
PolyOne Nymax™ GF 1200 A 33 HS Black 22 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Modulus | 8.62 - 11.9 GPa | 1250 - 1730 ksi | Average value: 9.85 GPa Grade Count:3 |
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | 8.62 - 16.2 GPa | 1250 - 2350 ksi | Average value: 12.5 GPa Grade Count:17 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF33 L NAT004 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: Natural ColorTPCI# 9411102Informatio.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF33 L UV BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and UV Stabilizer Features: Lubricated and Good UV ResistanceAppeara.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Techmer ES Luriblend® PC CF15 TL6 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF33 L NAT024 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: Natural ColorTPCI# 8221102Informatio.. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX APS430 PPE+PPS (Asia Pacific) PPE + PPS GF 30%, FR V-0 |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Chase Plastics CP Pryme® N233GL (DAM) Nylon 6, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Chase Plastics CP Pryme® N333GL (DAM) Nylon 6 (Utility Grade), 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU)