Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.55 GPa | 950 ksi | Tangent; ASTM D790 |
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
PolyOne Nymax™ GMF 600 A 40 Natural Polyamide 6 (Nylon 6) The Nymax® 600 Series of mineral-reinforced nylon 6 compounds have been specifically developed to provide an excellent balance of physical property performance and durability, with improved surface.. |
|||
Flexural Modulus | 6.55 GPa @Temperature 149 °C |
950 ksi @Temperature 300 °F |
|
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Techmer ES HiFill® PA6 IM 0240 Impact Modified Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Impact ModifierFeatures: High Density and Impact ModifiedProcessing Method: Injection MoldingInform.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Techmer ES HiFill® POM CO GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Techmer ES Luriblend® PC CF10 TL10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+PS LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® 71MR Mineral-Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® 89MRGFHS Glass Fiber and Mineral Reinforced Nylon 6 (DAM) Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in ind.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-43FG-0410 43% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Aaron Industries AAROPRENE® G/MFN 6002 Glass and Mineral Filled Nylon 6 AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133GTL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |