Plastics Group Polifil® 89MRGFHS Glass Fiber and Mineral Reinforced Nylon 6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® 89MRGFHS Glass Fiber and Mineral Reinforced Nylon 6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in industrial clamp components as well as bearings. Standard processing techniques are applicable.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Water Absorption 0.90 %
0.90 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength at Break 117 MPa
17000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 6.55 GPa
950 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Melting Point 218 °C
425 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149