Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.28 GPa | 621 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release. |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare. |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06408 PC LNP THERMOCOMP* DX06408 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC LNP* THERMOCOMP* DX06409 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon AD000Z ABS LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region... |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release |
|||
Flexural Modulus | 4.28 GPa | 621 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC (Asia Pacific) LNP* Thermocomp* DX06409 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |