Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.79 GPa | 550 ksi | Tangent; ASTM D790 |
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Oxford Polymers 10GF 10% Glass Fiber Reinforced Polyetherimide/Polycarbonate Alloy 10% Glass Fiber Reinforced Polyetherimide/Polycarbonate AlloyInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF17 IM2 L 17% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 17% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedInformatio.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES HiFill® HDPE GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF6 UG BK MB 6% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES Plaslube® J-50/10/TF/10 Polycarbonate, 10% GFR, 10% PTFE |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4731-13 Polycarbonate EMERGEâ„¢ PC 4731-13 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES Plaslube® J-50/10/TF/15 NAT Polycarbonate |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 3.79 GPa @Thickness 6.35 mm |
550 ksi @Thickness 0.250 in |
2.8 mm/min; ASTM D790 |
Chi Mei Kibisan® PN137H SAN Resin, General Purpose Information provided by Calsak Corporation |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Clariant PA123G20 Nylon 66, 20% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |