Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Nylene® Norpex® AX20MRFR , 20% Mineral Reinforced, Flame Retardant Polyphenylene Ether Description: Norpex® AX20MRFR is a 20% mineral reinforced, flame retardant PPE. AX20MRFR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all opertin.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
PolyOne Geon™ CPVC MC500 Polyvinyl Chloride, Chlorinated (CPVC) The Geon MC500 CPVC is an injection molding fittings compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon MC500 demonstrates superior processa.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Plaskolite Optix® DA Digital Acrylic Sheet Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Technetics Group Amicon™ PET-P
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Flexural Modulus | 3.38 - 11.7 GPa | 490 - 1700 ksi | Average value: 5.50 GPa Grade Count:4 |
Overview of materials for Polyphenylene Ether, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES HiFill® POM CO GC20 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 ML2 HS NAT Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(2%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizerAppear.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 ML2 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES HiFill® POM CO GC25 25% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 25% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Ensinger TECACRYL® TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to cr.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceExcellent clarityGood moldabilityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk organizersInfor.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Asahi Kasei Thermofil P-40MI-0600 40% Mica Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Asahi Kasei Thermofil P-40TC-8100 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PPX-MF-FR3 Modified PPO, UL 94 V-0 with HDT of 230 F, Mineral Reinforced
(Unverified Da Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |