Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.31 GPa | 480 ksi | Tangent; ASTM D790 |
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | Tangent; ASTM D790 |
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers PC-1010 Description: Polycarbonate, 10% Glass Filled BlackInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Oxford Polymers PEI 1010 PEI Product Description: (Unreinforced), Polyetherimide injection molding grade, high flow Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: .. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
PolyOne Edgetek® AS-10GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass/Carbon Fiber Filled
(discontinue Description/Features:Glass/Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Global GPC-FR-510 10% Glass Filled Flame Resistant Polycarbonate Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | |
Ineos Styrenics Polystyrene 168M0 (NAFTA) High heat, high molecular weight general purpose polystyrene with low residual volatiles. It is ideally suited for use in critical low taste, low odor food packaging products.Information provided b.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 ML2 HS BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Blac.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 ML2 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 1600 GPPS Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 3190/3191 GPPS Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Styrolution PS-168MO Polystyrene Description: Polystyrene 168MO is a high heat, high molecular weight general purpose polystyrene with low residual volatiles, excellent clarity and high melt strength. These properties makes it an e.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC310GR Polycarbonate (Utility Grade), 10% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Informat.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007F Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007F is a 40% talc filled homopolymer polypropylene compound that utilizes FDA compliant raw materials.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa @Temperature 22.8 °C |
480 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECAPEI® made from Ultem® 1000 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Americas Styrenics MC3700 High Heat Crystal Polystyrene Product CharacteristicsEasy filling of thin-walled partsExceptional mold releaseImproved cycle times in hard to fill partsFood Contact CompliantUL Classification 94HBUSP Class VITypical Applications.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | Tangent; ASTM D790 |
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |