Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.70 GPa | 392 ksi | |
Plastcom SLOVAMID 66 FRC 2 PA66, basic type FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. Used in automotive, electrical, engineering and co.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | |
Plastcom SLOVAMID 66 FRC 3 PA 66 basic type with flame retardant Features: Modified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. Used in automotive, electrical, engineering and .. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Flexural Modulus | 2.70 - 3.30 GPa | 392 - 479 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Flexural Modulus | 2.70 - 3.30 GPa | 392 - 479 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal .. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML4249 PC Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Transparent, transluscent and opaque colors. For blow molding. |
|||
Flexural Modulus | 2.70 - 12.0 GPa | 392 - 1740 ksi | Average value: 4.45 GPa Grade Count:6 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
Kolon KOCETAL® K900 Standard Grade Acetal Resin Very low viscosity grade. Applications: Thin and large products.Information provided by API-Kolon. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
IRPC Polimaxx Polene 2311NCX TA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 20% TALCUM REINFORCED, HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178 |
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178-93 |
Wellman Wellamid® NY1875-BK1 Nylon 66, Unfilled All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM-D790 |
Polyram RamTal PM7002 Acetal, UV Stabilized UV stabilized acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D 790 |
Cossa Polimeri ESTADIENE 0820 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood impact resistance, stiffness, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 630 Nylon 6/6, Flow Enhanced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830LB Nylon 6 Basic Nylon 6, medium viscosity, lubricated black.Data provided by the manufacturer |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830SMS Nylon 6, MoS2 Filled Basic Nylon 6, medium viscosity, lubricated with Molybdenum Disulfide.Data provided by the manufacturer |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 606 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
PlastxWorld Veroplas PA2000 Nylon 6 general purpose, unfilled injection molding gradeInformation provided by PlastxWorld Inc. |