Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.48 GPa | 360 ksi | Tangent; ASTM D790 |
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet) Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. .. |
|||
Flexural Modulus | 2.48 - 10.3 GPa | 360 - 1500 ksi | Average value: 4.62 GPa Grade Count:97 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakage.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
KYDEX® XD 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses Features:Tough and durableResistant to cracking and chippingSolid, integral color3500+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantExcellent fabrication qualit.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF14 IM4 HS L BKN 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Techmer ES Electrablend® PC 04007 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX11408 PC LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility |
|||
Flexural Modulus | 2.48 GPa | 359 ksi | ASTM D790 |
Spartech CastAlloy Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON AD000 ABS LNP* STAT-KON* AD000 is a compound based on ABS containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1453 Calcium Carbonate Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1453 is a long term heat aging grade of 40% calcium carbonate filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS/PA 1700 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Polimeri Europa SINKRAL L320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an .. |