Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
Oxford Polymers Oxnilon 6-60GF(DRY) PA6, 60% Glass Fiber Reinforced, Dry Product Description: Glass Fiber (60% Reinforced), Nylon 6 injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents, Lubricants and Heat Stabiliz.. |
|||
Flexural Modulus | 16.2 GPa @Temperature 115 °C |
2350 ksi @Temperature 239 °F |
ASTM D790 |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific) Thermally conductive electrically insulative mineral filled PPS FR compound. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP SCP36 PA12 LNP* LUBRICOMP* SCP36 is a compound based on Nylon 12 containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 C20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 CF20 L 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Semi Conductive and LubricatedInformation provided by TP C.. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 CF20 L BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP VERTON MV00ES PP LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
Techmer ES HiFill® PPS F GF/M55 BK 55% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
Techmer ES HiFill® PPS GF/M55 BK 55% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
Plenco 6401 Phenolic, Briquette, Transfer Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned Ultra high-rigidityInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 442 Glass Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 16.2 GPa | 2350 ksi | ASTM D570 |
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer
(discontinued **) XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe.. |
|||
Flexural Modulus | 16.2 - 16.2 GPa @Temperature 115 - 115 °C |
2350 - 2350 ksi @Temperature 239 - 239 °F |
Average value: 9.03 GPa Grade Count:1 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |