Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.1 GPa | 1460 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR33 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | ISO 178 |
Nilit FRIANYL B63 GV40 Nylon 6 for injection molding, 40% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp RFL38 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL38 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON JX89626 PES LNP* STAT-KON* JX89626 is a compound based on Polyethersulfone containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East) LNP* VERTON* MV00ASXC is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | ISO 178 |
Polyplastics FR-PET® CN9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | ISO 178-93 |
Wellman Wellamid® FRGFT1741-BK2 Nylon 66, 32% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | ISO 178-93 |
Wellman Wellamid® GFX1872-N1 (PTFE) Nylon 66, 33% Glass Reinforced, Lubricated All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | ISO 178-93 |
Wellman Wellamid® MRGF25/15 42H-BK167A Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced GM 167A Black color matchAll information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | ISO 178 |
Polyplastics Duranex® 750LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation .. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 656 Nylon 6/6, Carbon/Glass Fiber Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.1 GPa | 1460 ksi | |
Plastcom SLOVALEN PH 49 GF 60 PP reinforced with 60% glass fibre Features: Modified homopolymer PP for injection moulding, chemically reinforced with 60% glass fibre, contains the modifier of mechanical properties.Very good strength and tensile modulus. Delivered.. |
|||
Flexural Modulus | 10.1 GPa | 1470 ksi | 5 mm/min; ISO 178 |
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |