Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.25 GPa | 181 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 83 T 30 Polypropylene reinforced with mineral filler Impact modified PP for injection molding with the content of 30 % mineral filler. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers 1391 Polypropylene, Non-filled, Compounded Description: 1391 is a non-filled compounded polypropylene produced for automotive applications.Key Applications: Automotive exteriorInformation provided by Mytex Polymers |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Polimeri Europa Eraclene® MR 80 High Density Polyethylene - Injection Molding Eraclene MR 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. Eraclene MR 80 shows a good balance between processability and mechanical p.. |
|||
Flexural Modulus | >= 1.25 GPa | >= 181 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4052U (52411) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 1.25 GPa | >= 181 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1452S (H39S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Polimeri Europa Eraclene® MQ 70 U High Density Polyethylene - Injection Molding Eraclene MQ 70 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a mediu.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Regulatory StatusThe base resin LR 7320 meets t.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
LyondellBasell Petrothene® LR732013 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
LyondellBasell Petrothene® LR732031 High Density Polyethylene ApplicationsPETROTHENE LR 7320-31 is a high density polyethylene resin that exhibits an excellent balance of stiffness and environmental stress crack resistance. This resin has outstanding extrusio.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
LyondellBasell DEXFLEX® 727 TPO Description: DEXFLEX® 727 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, good low-temperature impact resistance.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer (Europe-Africa-Middle East) Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5740 UA HDPE Injection Molding Applications:Large dustbins and pailsPallet boxesFish cratesTechnical moldingInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | 2mm/min; ISO 178 |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR110MC2 is a metallocene random copolymer with a melt flow index of 110 g/10 min for injection molding. This Lumicene® MR110MC2 high fluidity differs from standard random copolymers by .. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total Lumicene® MR30MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR30MC2 is a metallocene random copolymer with a melt flow index of 30 g/10 min for injection molding. Lumicene® MR30MC2 differs from the other random copolymers by its molding reproduci.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPH 9082 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9082 is a controlled-rheology and antistatic homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing impr.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 179 |
Total PPM H250 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H250 is a narrow molecular weight distribution homopolymer with a Melt Flow Index of 25 g/10 min recommended for the manufacture of medical packaging and medical devices, to the ex.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Borealis RD360MO Polypropylene Random Copolymer, Transparent RD360MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleating and ant.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 503 Polypropylene Impact Copolymer Made for injection molding applications. Basic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPC 3640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3640 is a nucleated heterophasic copolymer. PPC 3640 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3640 has been devel.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
Entec Hypel® PEHD8/.953 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Modulus | 1.25 GPa | 182 ksi | 0.079 in/min; ISO 178 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips Marlex® 9708 HDPE Injection Molding Resin Resin Type: Linear Homopolymer; ASTM D 4976 Classification: PE 243, A 63700Characteristics: Moderate Flow, Good Impact Strength, Excellent Stiffness, Good ESCR, Moderate Shrinkage ResistanceApplicat.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | 1% secant; ASTM D790 |
Braskem H 504 XP Bioriented Film Polypropylene Description: H 504XP is a low melt flow rate homopolymer, designed specially for high speed lines of biorented films (BOPP). This product features a broad processing window with high output and regu.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | SAE J949 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | >= 1.25 GPa | >= 181 ksi | ISO 178 |
AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total Finathene® SI 508 HDPE blow molding
(discontinued **) Finathene® SI 508 is part of a new generation of high density ethylene-hexene copolymers produced by the slurry loop low pressure polymerization process. Finathene® SI 508 is a high molecular weig.. |