Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR120CL Polypropylene, Random Copolymer, Clarified, Lubricated Random clarified copolymer specially formulated to achieve high clarity and excellent color and color stability with excellent mold release properties. Applications: Injection molding applications s.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXFLEX® 990 TPO
(discontinued **) Description: DEXFLEX® 990 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, and excellent pr.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP400 Polypropylene Copolymer Features: Medium Flow, High Impact ResistanceUses: Appliances, Business Equipment, Construction Applications, Tool/Tote Box, ToysProcessing Method: Injection MoldingInformation provided by M. Hollan.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
LyondellBasell Petrothene® LP5100 High Density Polyethylene ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790A |
Ineos N00G-01 Polypropylene Impact Copolymer Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impa.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® A 9002 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Techmer ES Electrablend® ABS 03106 MB Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech Marballoy Marbleized Thermoplastic Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 3312E Random Copolymer Polypropylene Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3312E is a clarified, medium flow random copolymer with fast cycle time and easy mold release. It is designed for injection .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | |
CMW® ELKONITE® 40W3 Infiltrated Tungsten Copper material ASTM B702 For vacuum switch contacts, low expansion structural members.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11 Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | Tangent Method 1; ASTM D-790 |
Bapolene® 2035 Polyethylene, Blow Molding Grade Bapolene HD2035 is a high density polyethylene copolymer for blow molding applications. It is recommended for applications that require high top load strength and good ESCR properties. This produc.. |