Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.05 GPa | 152 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PC 69 T 10 003 Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | Tangent; ASTM D790 |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6750H (506H8) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1362R (Z21S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4310M (EP1X30F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
SABIC BM1052 High Density Polyethylene for Blow Molding Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | Tangent; ASTM D790 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790A |
Ineos L40N-00 Polypropylene Impact Copolymer L40N-00 is a nucleated high flow polypropylene, medium impact copolymer for injection molding applications. This resin exhibits an excellent balance of resin flow and mechanical properties. This res.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790A |
Ineos R35C-02 Polypropylene Random Copolymer Grade R35C-02 is a high clarity, lubricated random copolymer with a high flow rate. This material is designed for high-speed injection molding of medium- to thin-walled parts requiring excellent cla.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem HC 7260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem HC 7260 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Iran Petrochemical (PCC) 5218EA High Density Polyethylene HD-5218EA is a high density polyethylene copolymers containing butane-1 as the comonomer with narrow molecular weight distribution, suitable for thin wall injection application. It has been designed.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Iran Petrochemical (PCC) EPD 60 R Polypropylene EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include t.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | |
Kraton® D1102 + PP blend (25/75) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5226 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EE040AE TPO Compound Daplen EE040AE is an elastomer modified polypropylene compound intended for injection molding. Daplen EE040AE is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansi.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EF040AE TPO Compound Daplen EF040AE is a elastomer modified polypropylene compound intended for injection molding. Daplen EF040AE is a material with excellent impact/stiffness ratio. Thanks to its low thermal expansio.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 805 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 1.0 in/min; 0.125" thickness; ASTM D-790 |
Chevron Phillips K-Resin® XK44 SBC K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Thermoformed clam shell packagingThermoformed blister packsThermoformed medical traysBlow molded productsFeatures:Good clarityGood stiffnessGo.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | Chord, 0.079 in/min; ISO 178 |
ExxonMobil Exxtral™ H1025 Performance Polyolefin Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.Availability.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QW 73 AV Propylene Random Copolymer Description: CAPILENE® QW 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QW 73 AV is clarified with antista.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, Conditioned Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QT 73 A Propylene Random Copolymer Description: CAPILENE® QT 73 A is a clarified and antistatic additivated polypropylene random copolymer with a high melt flow rate, intended for injection molding of clear articles. It exhibits g.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QU 73 AV Propylene Random Copolymer Description: CAPILENE® QU 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QU 73 AV is clarified with antista.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, Conditioned Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |