Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.790 GPa | 115 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9301 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234360A; ASTM D 4976 Classification: PE 225, A 56607Applications:Base Resin for use in Gas, Oil Patch and Industrial Pipe.. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9302 HDPE Yellow Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607Applications:Natural Gas Distribution Piping and FittingsData provide.. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 7040 G HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ISO 178 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ISO 178 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ISO 178 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP) LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ASTM D790 |
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6 26% crystallinity. Information supplied by Elastomer Engineering. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | ASTM D790 |
Asahi Glass Fluon® AH-2000 LM-ETFE, Non-Conductive Type, Fluororesin Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive ag.. |
|||
Flexural Modulus | 0.790 GPa | 115 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
LyondellBasell DEXFLEX® 810-1 TPO Description: DEXFLEX® 810-1 is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. DEXFLEX® 810-1 was designed to exceed the requiremen.. |