| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade |
| Manufacturer | Elastomer Engineering |
| Trade Name | Elastamide |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Water Absorption | 2.4 % | 2.4 % | 24 hrs; DIN 53714 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 66 | 66 | |
| Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
| Elongation at Break | 400 % | 400 % | ASTM D638 |
| Tensile Modulus | 0.650 GPa | 94.3 ksi | ASTM D638 |
| Flexural Modulus | 0.790 GPa | 115 ksi | ASTM D790 |
| Shear Modulus | 0.400 GPa | 58.0 ksi | Torsional |
| Izod Impact, Notched | 9.02 J/cm | 16.9 ft-lb/in | Method B; Ductile Failure |
| 1.23 J/cm @Temperature -40.0 °C |
2.30 ft-lb/in @Temperature -40.0 °F |
Method B; Brittle/Ductile Failure | |
| Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Ductile Failure; ASTM D256B |
| 0.550 J/cm² @Temperature -40.0 °C |
2.62 ft-lb/in² @Temperature -40.0 °F |
Method B; Brittle Failure | |
| Taber Abrasion, mg/1000 Cycles | 8.0 | 8.0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 4.3 @Frequency 100000 Hz |
4.3 @Frequency 100000 Hz |
|
| 7.9 @Frequency 1000 Hz |
7.9 @Frequency 1000 Hz |
||
| 14.9 @Frequency 50 Hz |
14.9 @Frequency 50 Hz |
||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | |
| Dissipation Factor | 0.10 @Frequency 100000 Hz |
0.10 @Frequency 100000 Hz |
ASTM D150 |
| 0.30 @Frequency 1000 Hz |
0.30 @Frequency 1000 Hz |
ASTM D150 | |
| Comparative Tracking Index | 500 V | 500 V | ASTM D257 |