Dart Drop, Total Energy 19.0 J

@Temperature -30.0 °C
14.0 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS
PC+ABS Blend with 20% Glass Reinforce. High heat resistance; Excellent balance strength/rigidity; Good impact/appearance.
Dart Drop, Total Energy 19.0 J

@Temperature 0.000 °C
14.0 ft-lb

@Temperature 32.0 °F
Instrumented Impact Energy @ peak, @ 6.6 m/s; ASTM D3763
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP
SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili..
Dart Drop, Total Energy 19.0 J

@Temperature -30.0 °C
14.0 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak, -30°C @ 6.6 m/s; ASTM D3763
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP
SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st..
Dart Drop, Total Energy 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP
SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st..
Dart Drop, Total Energy 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP
SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st..
Dart Drop, Total Energy 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP
30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited).
Dart Drop, Total Energy 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Asia Pacific)
30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited).
Dart Drop, Total Energy 19.0 J

@Temperature -20.0 °C
14.0 ft-lb

@Temperature -4.00 °F
ASTM D3763
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin
Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is..
Dart Drop, Total Energy 19.0 J

@Temperature 22.8 °C
14.0 ft-lb

@Temperature 73.0 °F
ASTM D3763
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin
Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos..
Dart Drop, Total Energy 19.0 J

@Temperature 22.8 °C
14.0 ft-lb

@Temperature 73.0 °F
ASTM D3763
ExxonMobil Escorene™ LD 705.MJ Blown Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 705.MJ is a fractional melt index, 12.8 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and..