Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 1600 MPa @Temperature 23.0 °C |
232000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa @Temperature 23.0 °C |
232000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa @Temperature 23.0 °C |
232000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa | 232000 psi | |
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa @Time 3.60e+6 sec |
232000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring .. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa @Temperature 23.0 °C |
232000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa @Time 3.60e+6 sec |
232000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear .. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa @Time 3.60e+6 sec |
232000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa | 232000 psi | |
BASF Polystyrol® 445 E WU Impact Grade Polystyrene (Europe) Easy flowing, heat-resistant, medium-impact, flame-retardant grade. Application example: electrical distribution boxes.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa | 232000 psi | |
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe) Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa | 232000 psi | |
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade
(discontinued **) OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall.. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa @Strain <=0.500 % |
232000 psi @Strain <=0.500 % |
ISO 899-1 |
Styrolution Luran® S KR 2861/1 C Colored ASA+PC Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh.. |
|||
Tensile Creep Modulus, 1000 hours | 1600 MPa | 232000 psi | ISO 899-1 |
Lanxess Pocan® S 7020 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |