Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 520 MPa | 75400 psi | |
Arkema Group Orgalloy® LE 6000 Nylon Alloy, Flexible Grade (Conditioned) LE series, flexible polyamide alloys: processable on PE screws, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the extrusion of .. |
|||
Tensile Creep Modulus, 1000 hours | 520 MPa | 75400 psi | |
Arkema Group Orgalloy® LE 6000T Nylon Alloy, Flexible Grade (Conditioned) LE series, flexible polyamide alloys: processable on PE screws, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the extrusion of .. |
|||
Tensile Creep Modulus, 1000 hours | 520 MPa | 75400 psi | |
Arkema Group Orgalloy® LE 60ES03 Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in viscosity than LE 6000, suited to the blow molding of tec.. |
|||
Tensile Creep Modulus, 1000 hours | 520 MPa | 75400 psi | |
Arkema Group Orgalloy® LE 60ES Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in viscosity than LE 6000, suited to the blow molding of tec.. |