Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.310 GPa | 45.0 ksi | ASTM D882 |
Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, High Slip, Very High Antiblock Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit.. |
|||
Secant Modulus, TD | 0.310 GPa | 45.0 ksi | ASTM D882 |
Chevron Phillips 7109DT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, No Slip, No Antiblock Version of 7109T with Process Aid, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or ble.. |
|||
Secant Modulus, TD | 0.310 GPa | 45.0 ksi | ASTM D882 |
Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, High Antiblock Version of 7109TCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPEApplications:Ind.. |
|||
Secant Modulus, TD | 0.310 GPa | 45.0 ksi | ASTM D882 |
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags.. |
|||
Secant Modulus, TD | 0.310 GPa | 45.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 14K1 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.310 GPa | 45.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.310 GPa | 45.0 ksi | ASTM D882-A |
Borealis Borstar® FB4250T LLDPE for Blown Film Borstar FB4250 is well suited for a wide range of film applications due to its properties. The well balanced mechanical properties will improve the functionality of the films or allow for material .. |
|||
Secant Modulus, TD | 0.310 - 0.520 GPa | 45.0 - 75.4 ksi | Average value: 0.417 GPa Grade Count:15 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |