Mechanical Properties Metric English Comments
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Slip, Very High Antiblock Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
Chevron Phillips 7109D Linear low density polyethylene blown film resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymer, no slip, no antiblock version of 7109 with process aid, cast/blown resinCharacteristics: good stiffness at thin gauges, good drawdown, ..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film
Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film
Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882-A
Borealis Borstar® FB4250T LLDPE for Blown Film
Borstar FB4250 is well suited for a wide range of film applications due to its properties. The well balanced mechanical properties will improve the functionality of the films or allow for material ..
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
DuPont™ Surlyn® 1601B-2 Sodium Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1601 B-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry,..