Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 58.0 - 70.0 MPa | 8410 - 10200 psi | IS 867-1963 |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Shear Strength | 67.0 - 70.0 MPa | 9720 - 10200 psi | IS 867-1963 |
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Shear Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | IS 867-1963 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Shear Strength | 55.0 - 70.0 MPa | 7980 - 10200 psi | IS 867-1963 |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Shear Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | IS 867-1963 |
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha.. |