Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 52.0 MPa | 7540 psi | |
Pyrotek F-24 Dense Machinable Board F-24 is a high temperature resin material that is reinforced with fiberglass. Abrasion resistant, it is used for hot glass handling applications.ApplicationsDonut rollers for glass Guide rails Wear.. |
|||
Shear Strength | 52.0 MPa | 7540 psi | Shear Bond Holding Strength |
Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation. |
|||
Shear Strength | 52.0 MPa | 7540 psi | |
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation |
|||
Shear Strength | 52.0 MPa @Temperature 75.0 °C |
7540 psi @Temperature 167 °F |
In-Plane, Wet; EN6031 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |
|||
Shear Strength | 52.0 MPa | 7540 psi | T300 (6K); Short Beam; [0°]16 |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |
|||
Shear Strength | 52.0 MPa | 7540 psi | T300 (6K); Short Beam; [0°]16; Wet Condition |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |