Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 45.0 MPa | 6530 psi | In-Plane |
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M60J Fiber Information provided by HexCel |
|||
Shear Strength | 45.0 MPa | 6530 psi | In-Line; ASTM D5379 |
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite HexMC® is a high performance carbon molding composite, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume content enable components to be molded for a wide.. |
|||
Shear Strength | 45.0 MPa | 6530 psi | I.L.S.S. short beam shear per ASTM D5379 |
Hexcel® HexMC™ C / 2000 / R1 Composite SMC High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications.. |
|||
Shear Strength | 45.0 MPa @Temperature 100 °C |
6530 psi @Temperature 212 °F |
0º, ILSS (Short Beam), Wet; EN2563 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |
|||
Shear Strength | 45.0 MPa @Temperature 100 °C |
6530 psi @Temperature 212 °F |
In-Plane, Wet; EN6031 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |
|||
Shear Strength | >= 45.0 MPa | >= 6530 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe. |
|||
Shear Strength | 45.0 MPa @Temperature 80.0 °C |
6530 psi @Temperature 176 °F |
Warp ILSS |
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26/45%/G1070 Carbon Fabric 6K T300J 370 gsmInformation provided by HexCel |