Polymer Property : Shear Strength = 52.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 52.0 MPa
7540 psi
Pyrotek F-24 Dense Machinable Board
F-24 is a high temperature resin material that is reinforced with fiberglass. Abrasion resistant, it is used for hot glass handling applications.ApplicationsDonut rollers for glass Guide rails Wear..
Shear Strength 52.0 MPa
7540 psi
Shear Bond Holding Strength
Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy
Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation.
Shear Strength 52.0 MPa
7540 psi
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy
Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation
Shear Strength 52.0 MPa

@Temperature 75.0 °C
7540 psi

@Temperature 167 °F
In-Plane, Wet; EN6031
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel
Shear Strength 52.0 MPa
7540 psi
T300 (6K); Short Beam; [0°]16
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form
Fiber: T300-12K, IM7-12KInformation provided by HexCel
Shear Strength 52.0 MPa
7540 psi
T300 (6K); Short Beam; [0°]16; Wet Condition
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form
Fiber: T300-12K, IM7-12KInformation provided by HexCel