Mechanical Properties Metric English Comments
Shear Strength 4.48 MPa

@Treatment Temp. 21.0 °C,
Time 86400 sec
650 psi

@Treatment Temp. 69.8 °F,
Time 24.0 hour
Lap
Parker Chomerics CHO-BOND 584-29 Conductive Adhesive
Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m..
Shear Strength >= 4.48 MPa
>= 650 psi
Parker Chomerics CHO-BOND 589-29 Conductive Epoxy
Low cost, highly conductive adhesive system which combines the strong adhesion characteristics of an epoxy with the superior conductivity of silver. CHO-BOND 589-29 adhesive meets the most exacting ..
Shear Strength 4.48 - 35.2 MPa
650 - 5100 psi
Average value: 14.2 MPa Grade Count:58
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Shear Strength >= 4.48 MPa
>= 650 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR III 1/4-5052-.004 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 4.48 MPa
650 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP - 3/16 - 7.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength >= 4.48 MPa
>= 650 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 4.48 MPa
650 psi
Overlap, Aluminum; ASTM D1002-64
3M Scotch-Weld™ CA5 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity, slower setting version of CA4 for filling gaps. Meets CID A-A-3097, Type II, Clas..
Shear Strength 4.48 MPa
650 psi
Overlap, ABS, Adhesive/Cohesive Failure
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 4.48 MPa
650 psi
Tensile Shear Adhesion, on a grit blasted steel
3M Scotchkote™ SG 527 Epoxy Metal Repair
Scotchkote Epoxy Metal Repair SG 527 is a specially packaged rapid curing synthetic metal repair compound for on site repairs to metal components such as leaking pipes, tanks, ducts, and radiators.P..
Shear Strength 4.48 MPa
650 psi
Overlap, Glass (3/16" thick), Substrate Failure
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 4.48 MPa

@Temperature 149 °C
650 psi

@Temperature 300 °F
Etched Aluminum Overlap
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
Shear Strength 4.48 MPa
650 psi
Overlap, Wood, Fir
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M
Shear Strength 4.48 MPa
650 psi
Overlap, PVC
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M