Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ND Industries 301 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ND Industries 306 Surface Insensitive Instant Superglue Low viscosity for difficult to bond rubber compounds |
|||
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ND Industries 331 Surface Insensitive Instant Superglue Medium-high viscosity for difficult to bond surfaces |
|||
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ND Industries 333 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ND Industries 360 Surface Insensitive Instant Superglue General DescriptionA medium viscosity, general purpose cyanoacrylate which is also surface sensitive. Can handle a wide array of materials which include wood, cork, leather, stone and plastics, in .. |
|||
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ND Industries SuperGlue Ethyl 314 General DescriptionA medium viscosity ethyl-based cyanoacrylate particularly suitable for rubbers and plastics. It is fast acting and may be fillet cured using ND Excel Accelerators.rubber O-rings,.. |
|||
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ND Industries SuperGlue Ethyl 316 Medium-high viscosity for gap fillingMeets military spec Mil-A-46050C Type II Class III |
|||
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ND Industries SuperGlue Ethyl 344 Medium viscosity, general purposeMeets military spec Mil-A-46050C Type II Class III |
|||
Shear Strength | 20.7 MPa | 3000 psi | |
NextGen Adhesives G907-21 Structural Epoxy Adhesive Description: NGAC G907-21 is a high viscosity and thixotropic adhesive system that is specifically formulated for structural bonding applications: industrial, electronics and aerospace.Advantages an.. |
|||
Shear Strength | 20.7 MPa | 3000 psi | |
Indium Corp. Indalloy 149 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
ITW Plexus Plexusâ„¢ MA310 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with "difficult to bond" plastics, high strength.Information provided by Illinois Tool Works. |
|||
Shear Strength | >= 20.7 MPa | >= 3000 psi | Bond, Al to Al |
Master Bond EP30HT-LO NASA Low Outgassing, Optically Clear Coating Description: Master Bond EP30HT-LO is a moderate viscosity, two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio.. |
|||
Shear Strength | 20.7 MPa | 3000 psi | |
Trelleborg Emerson & Cuming Syntac® 350 Composite Materials Syntactic Foam Syntac 350 foam is a rigid, high strength composite of epoxy resin and microscopic hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling. .. |
|||
Shear Strength | 20.7 MPa | 3000 psi | |
Dymax Magnet Bonder™ 2020 Adhesive DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2020 Magnet Bonder™ AdhesiveAcrylic and methacrylic acid-free; bond ferrite to metal, plated metals, E-coat, sealed cans.. |
|||
Shear Strength | 20.7 MPa @Temperature 24.0 °C |
3000 psi @Temperature 75.2 °F |
Aluminum Overlap; ASTM D1002 |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Shear Strength | 20.7 MPa @Temperature -55.0 °C |
3000 psi @Temperature -67.0 °F |
Overlap |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Shear Strength | 20.7 MPa | 3000 psi | Overlap, Water Vapor, 93°C at 100% RH for 14 days |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 20.7 MPa | 3000 psi | Overlap, Galvanized Steel Okite degrease Electrodeposited |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 20.7 MPa @Temperature -55.0 °C |
3000 psi @Temperature -67.0 °F |
Etched Aluminum Overlap |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |
|||
Shear Strength | 20.7 MPa | 3000 psi | ASTM D1002-94 |
Aremco Aremco-Bond™ 631 High Performance Epoxide Clear-Amber, 1:1, Good Bond Strength and Corrosion Resistance.Also available filled with aluminum oxide (Alumina) or pigments. |
|||
Shear Strength | 20.7 MPa | 3000 psi | cured, grit-blasted steel; ASTM D1002 |
3M Scotch-Weld™ EC600 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Shear Strength | 20.7 MPa @Temperature -73.0 °C |
3000 psi @Temperature -99.4 °F |
Overlap, Etched Aluminum; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 20.7 MPa @Temperature -53.0 °C |
3000 psi @Temperature -63.4 °F |
Overlap, Etched Aluminum; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 20.7 MPa | 3000 psi | Overlap, Etched Al, Hydrocarbon Fluid for 7 days |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 20.7 MPa @Temperature -53.0 °C |
3000 psi @Temperature -63.4 °F |
Overlap, Etched Aluminum; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 20.7 MPa | 3000 psi | Overlap, Antifreeze/H2O (50/50) immersion, 82°C for 30 days |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 20.7 MPa | 3000 psi | |
Dymax Magnet Bonder™ 2010 Adhesive DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2010 Magnet Bonder™ AdhesiveHigh performance; bond plated materials, E-coat Typical Use: D.C. motor magnet to can bond.. |