Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
ND Industries 560 Shaft & Bearing Retainer Retaining Compound High Temperature retainer for bushings and sleeves. Retains rotors to shaftsMeets military spec Mil-R-46082B Type II |
|||
Shear Strength | 13.8 MPa | 2000 psi | Tensile |
Resin Technology Group UV-S-2051 High Impact, UV Curable Plastic Bonder UV S-2051 is a general purpose, fast cure response, high thermal-shock resistant, UV curing adhesive designed for use in a variety of applications including chip bonding, laminating, tacking, and se.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | |
NextGen Adhesives G907-08 Epoxy Adhesive Description: NGAC G907-08 is a low viscosity, electrically insulating, heat cured and 2-part adhesive systems designed for applications where temperature and chemical resistance is critical. The NGA.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | |
Indium Corp. Indalloy 13 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile lap, Al/Al |
Master Bond EP42HT-2ND-2Med Heat Resistant, Medical Grade Non-Drip Epoxy Master Bond Polymer System EP42HT-2ND2MED (Black) is a room temperature curable two component epoxy adhesive and sealant featuring high temperature resistance along with outstanding chemical resista.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Bond, Al to Al |
Master Bond EP77M-1 Fast Setting, Silver Conductive Epoxy Description: Master Bond Polymer System EP77M-1 is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile lap, Al/Al |
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 320-3 Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 323LP Epoxy Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 353ND-T4 Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T4 is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. This is a higher viscosity version of EPO-TEK® 353.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® E3035 Electrically Conductive Adhesive Product Description: EPO-TEK® E3035 is a single component, silver-filled epoxy for hybrid die and component attach.Advantages & Application Notes: Performs exceptionally well as a die attach for sm.. |
|||
Shear Strength | 13.8 - 15.2 MPa | 2000 - 2200 psi | CRS Overlap |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, Steel; ASTM D1002-64 |
3M Scotch-Weld™ CA8 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting than CA7 and excellent adhesion to metals, and plastics and rubbers. Meets CID A-A-3.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, Galvanized Steel Hot dipped |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 13.8 MPa @Temperature -55.0 °C |
2000 psi @Temperature -67.0 °F |
Overlap, Etched Aluminum |
3M Scotch-Weld™ DP807 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT40 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Lap, Alum to Alum |
Atom Adhesives AA-BOND FDA15 Epoxy Adhesive AA-BOND FDA15 is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administr.. |
|||
Shear Strength | 13.8 MPa @Temperature 33.0 - 36.0 °C |
2000 psi @Temperature 91.4 - 96.8 °F |
Etched Aluminum Overlap, Salt Spray Immersion for 250 hrs, Minimum MIL-A-8623 Type III Requirement |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 13.8 MPa | 2000 psi | |
Dymax Magnet Bonder™ 2000 Adhesive DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2000 Magnet Bonder™ AdhesiveFastest cure; bond ferrite to steel. Typical Use: Loudspeaker magnet to pole piece. |
|||
Shear Strength | 13.8 MPa @Temperature -53.0 °C |
2000 psi @Temperature -63.4 °F |
Overlap, Etched Aluminum; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Bond, Al to Al |
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig.. |